The fracture conduct and fracture manner in the diffusion-bonded joints were being elucidated by macro fracture and magnified surface morphologies. The macro fracture morphologies (flat fracture) display which the propagation of crack occurred alongside the MEA/DD5 interface in tensile checks from the joints reached at 1020, 1050, and 1080 °C (Fig